Leave Your Message
Copper Based Pre-alloyed Powder

Superfine Pre-alloyed Powder

Copper Based Pre-alloyed Powder

Copper Based Pre-alloyed Powder KIN-01
Copper Based Pre-alloyed Powder SCF-11

Has good self sharpening ability, making easier protrusion during cutting and grinding processes. 

Suitable for low-temperature sintering, the best sintering temperature is between 650-800℃.

    Features

    With characteristics of good holding force to diamonds, faster protrusion of diamond grit and long time for grinding and cutting.

    Application

    Copper based formula alloyed powder for glass, rock slab and concrete.
    • metal powder for glass drill bitwto
    • metal powder for grinding wheelgpo
    • metal powder for diamond toolsxf5

    Data

    Grade

    Composition

    Particle Size
    D50(μm)

    Hardness
    (HRB)

    Bending Strength
    (MPa)

    Apparent Density
    (g/cm3)

    Theoretical Density
    (g/cm3)

    KIN-01

    Cu Co Sn Zn

    8.0-15.0

    84-90

    800-950

    2.3-2.8

    8.58

    SCF-11

    Cu Fe Sn P

    10.0-15.0

    80-90

    800-1000

    2.0-2.6

    8.21

    The above product data and application suggestions may change due to product optimization, performance improvement, and other reasons. The current content is for reference only. Please contact us for the latest data.